New tungsten carbide grade enhances cutting tool performance for superalloy machining

WORTHINGTON, Ohio, Sept. 18, 2025 (GLOBE NEWSWIRE) -- Hyperion Materials & Technologies, a leading global hard materials company, today announced the launch of grade AM10F tungsten carbide rod tool blanks that raise the bar for machining heat-resistant superalloys (HRSAs) and other advanced materials.

Engineered for high-performance round tools used in aerospace, energy, marine, and other demanding industries, carbide grade AM10F exhibits increased wear resistance that keeps cutting edges sharper longer to allow manufacturers to maximize production efficiency and reduce scrap costs.

“We work continuously with our toolmaking and manufacturing partners to achieve optimal solutions through longer, more consistent tool life,” said Biju Varghese, Hyperion Senior Vice President who oversees the company’s product management and research and development teams. “We’re excited to align the introduction of grade AM10F with EMO Hannover in Germany later this month, where we can connect with many of our current and prospective production technology partners.”

Hyperion tapped decades of hard materials expertise and tight manufacturing process controls to develop carbide rod blanks in grade AM10F to excel in tools used to cut HRSAs such as Inconel™, Monel™, René, Nimonic™, Hastelloy™, and Haynes™. In side milling tests performed on Inconel 718, Hyperion compared tool performance and reliability using carbide grade AM10F and two premium substrates from competitors. Tools made of AM10F lasted more than 50% longer with far greater tool life predictability. Material analysis revealed the more consistent microstructure and chemistry of AM10F translated to predictably long tool life.

“For customers that work with notoriously difficult-to-cut materials that wear out tools quickly and increase the risk of unexpected failures that can lead to scrapping high-value components, grade AM10F’s ability to deliver predictable results with cutting edges that break less often will be a game changer,” said Susanne Sowers, Research & Development Director who managed the development of the new product. “This is a market-leading product that will empower cutting-edge toolmakers to drive performance improvements that will increase productivity and cost savings for manufacturers.”

Carbide rod blanks in grade AM10F are the newest addition to Hyperion’s Application Specific series of carbide rods engineered for fabricating high-performance tools used to machine advanced materials. Carbide rod blanks in grade AM10F deliver:

  • Superior wear for enhanced resistance to chipping, making it the ideal substrate for high-performance cutting tools used in aerospace, energy, marine, and medical manufacturing
  • Predictably long tool life that minimizes unexpected failures and enhances productivity by allowing machines to run optimal parameters longer
  • High-quality material consistency to decrease blank inspection time and speed up tool production with carbide rods that consistently meet tight quality specifications
  • Extended tool life in demanding applications, reducing downtime, cost per part, and total cost of ownership

Carbide rod blanks in grade AM10F are available as solid rods in a variety of finishes in imperial and metric dimensions. Contact Hyperion to connect with a specialist who can recommend a range of standard and custom products.

About Hyperion Materials & Technologies

Hyperion Materials & Technologies, headquartered in Worthington, Ohio, USA, is a global leader in hard and super-hard materials with nearly 80 years of experience developing cemented carbide, diamond, and cubic boron nitride technologies. Hyperion supplies premium toolmaker components, engineered process solutions, and custom wear parts for the most demanding applications. Hyperion has production facilities in North and South America, Europe, and Asia; sales in more than 70 countries; and more than 2,200 employees worldwide.

To learn more, go to HyperionMT.com or visit Hyperion’s profiles on LinkedIn or YouTube.

Inconel, Monel, and Nimonic are registered trademarks of Special Metals Corp. or related entities in certain jurisdictions globally.

Hastelloy and Haynes are registered trademarks of Haynes International Inc. in certain jurisdictions globally.

A photo accompanying this announcement is available at https://www.globenewswire.com/NewsRoom/AttachmentNg/0e333e08-1cc3-4078-b013-5a8436702202


Media Contact

Matthew Seymour
Vice President of Marketing
matthew.seymour@hyperionmt.com

Primary Logo

Stock Quote API & Stock News API supplied by www.cloudquote.io
Quotes delayed at least 20 minutes.
By accessing this page, you agree to the following
Privacy Policy and Terms Of Service.


 

IntelligentValue Home
Close Window

DISCLAIMER

All content herein is issued solely for informational purposes and is not to be construed as an offer to sell or the solicitation of an offer to buy, nor should it be interpreted as a recommendation to buy, hold or sell (short or otherwise) any security.  All opinions, analyses, and information included herein are based on sources believed to be reliable, but no representation or warranty of any kind, expressed or implied, is made including but not limited to any representation or warranty concerning accuracy, completeness, correctness, timeliness or appropriateness. We undertake no obligation to update such opinions, analysis or information. You should independently verify all information contained on this website. Some information is based on analysis of past performance or hypothetical performance results, which have inherent limitations. We make no representation that any particular equity or strategy will or is likely to achieve profits or losses similar to those shown. Shareholders, employees, writers, contractors, and affiliates associated with ETFOptimize.com may have ownership positions in the securities that are mentioned. If you are not sure if ETFs, algorithmic investing, or a particular investment is right for you, you are urged to consult with a Registered Investment Advisor (RIA). Neither this website nor anyone associated with producing its content are Registered Investment Advisors, and no attempt is made herein to substitute for personalized, professional investment advice. Neither ETFOptimize.com, Global Alpha Investments, Inc., nor its employees, service providers, associates, or affiliates are responsible for any investment losses you may incur as a result of using the information provided herein. Remember that past investment returns may not be indicative of future returns.

Copyright © 1998-2017 ETFOptimize.com, a publication of Optimized Investments, Inc. All rights reserved.